How long will CUTEK® timber oil last? How often will I have to reapply?

CUTEK® timber oils should be reapplied when the wood is no longer beading or as frequently as necessary to retain the natural or altered colour of the wood. Timing will differ depending on many variables including the age and porosity of the wood, species, situation, design, aspect, weathered exposure and adequacy of preparation.

When considering frequency of maintenance there are two factors to consider:

  1. Protection: CUTEK® Extreme CD50 diffuse deeply into wood to provide, long-term, accumulative, inside out protection. Even when the timber surface has greyed and weathered, CUTEK® timber oils remain permanently mobile in the timber, meaning protection is not compromised even if the outward appearance of the wood has changed. Each additional coat of CUTEK® timber oil provides further additional protection against moisture.
  2. Appearance: To maintain the natural colour of freshly oiled wood for longer or alter the appearance of your timber, a CUTEK® oil with an added CUTEK® Colourtone should be applied. Over time and with exposure to sunlight and UV, the colour will slowly fade to a silver patina. Colour durability and the rate at which this fading occurs is dependent on many factors such as age and porosity of the wood, species, situation, design, aspect, and degree of exposure to the weather. CUTEK® timber oil should be reapplied as frequently as necessary to maintain desired colour vibrancy.

I applied a CUTEK® oil to my timber but it now has black spots?

When successfully applied, it is highly unlikely that CUTEK® timber oils will cause black spots to appear on timber. Commonly, there are two issues that could result in the appearance of black spots:

1. The presence of iron stain:

Iron stain, is an unsightly blue–black or grey discoloration that is often incorrectly described as “mould” because of its frequently “spotty” appearance. While iron stain can occur on nearly all timber species, some timbers are particularly prone to iron stain because they contain large amounts of tannin-like extractives that readily react with iron present in the environment to form insoluble stains.

The discolouration is often caused by a chemical reaction between extractives and iron content in steel products, such as nails, screws, and other fasteners. Iron contamination can also come from traces of iron left on wood from cutting, grinding or slicing; cleaning the surface with steel wool, wire brushes, or iron tools; using finishes stored in rusty containers; and using previous iron-containing or iron-contaminated finishes. Iron dust from metalworking and even plant fertilizers can be sources of iron along with removal of old rusted guttering, handrail construction and contact by steel capped boots.

2. Moisture content was too high when CUTEK® oil was applied:

Timber must be completely dry and non-greasy before applying CUTEK®; specifically the moisture content of the timber must be less than 17%. If CUTEK® is applied to timber with a moisture content greater than 17%, CUTEK® may sit on the surface and may rarely present with a dark blotchy discolouration (especially with colourtoned CUTEK®).

Rectifying both of these issues is a simple process. After the CUTEK® oil has been allowed to dry completely, wet the timber and apply undiluted CUTEK® Restore to the timber with a brush, roller or broom where discolouration exists. When the black spots/discolouration has disappeared, use a pressure washer to remove CUTEK® Restore (refer to the CUTEK® Restore label or Factsheet for further information). When the timber has dried (moisture content less than 17%), reapply your CUTEK® timber oil.

Understanding Colourtones

It’s important to understand that CUTEK® is a unique penetrating oil system designed to enhance the natural colour and grain of wood. CUTEK® is sold as a clear oil which can be used to protect the wood from moisture and moisture related movement such as cupping, warping and splitting. Using just the clear oil will protect the wood, providing stability and structural integrity while allowing it to naturally lighten to produce a silver weathered patina over time. The soft natural lightening and silvering of the wood represents a low care option and is becoming an increasingly popular way to leave wood in weather exposed settings.

Wood projects using clear CUTEK® oil that have silvered can easily be returned back to the wood’s original colour using CUTEK® Restore and high pressure washing followed by further applications of CUTEK® clear oil.

However, if you desire to maintain the original colour of the wood then you need to purchase a CUTEK® Colourtone suited to your selected wood which will further enhance the natural colour and grain and help to maintain its “natural” colour over a longer period of time.

NOTE: CUTEK® is unable to offer any specific performance warranties in relation to colour retention for CUTEK® products because of many variables related to the weathering process including but not limited to: the age and porosity of the wood, species, situation, design and structure, aspect, differing exposure to the weather, method of application and adequacy of preparation.

What to expect when using CUTEK® Colourtones

Most wood care products on the market leave a build up of material on the surface of the wood. In the short term this provides more colour, but in the long term the finish can be prone to peeling and flaking, which requires time and money to repair.

The CUTEK® system is unique as it will fade over time rather than peel or flake. The initial CUTEK® Colourtone build on new smooth wood projects only offers subtle amounts of pigment that enhance the wood. Timber that’s exposed fully to the weather will lighten faster as the wood acclimatises over the first six months. A follow up application after this initial weathering period will provide much greater Colourtone build as the wood becomes rougher and more open.

How to increase colour build on new wood

New wood is milled smooth and often has a mill glaze which will greatly restrict the initial colour build. Better results can be achieved by creating a rougher surface and preparing the wood using CUTEK® Restore in combination with a high pressure washer. Sanding the new wood to 80 grit will give even better results as it removes mill glaze and creates a much rougher surface which will enable higher colour build.

NOTE: The rougher the surface of the wood, the greater the colour build and durability. Rough sawn or heavy brushed wood profiles will take more oil and colour so much bolder colour contrast can be achieved. The amount of mill glaze if any that is present on any job can vary significantly depending on species density, and machining method used. Note, sanded surfaces should be vacuumed or washed thoroughly to remove all loose wood and dust.

Select CUTEK® Colourtone

Our CUTEK® Colourtone system is designed to enhance the wood colour and grain you select. With this in mind, you need to think about your original wood choice and the colour it most represents. Is it light to Golden, Brown, Red or a combination? Here are a few common examples to help you understand:

Black Butt and Silver Top Ash: Light tones so Rustic Gold is a good choice

Spotted Gum: Light creamy to brown and greys so Rustic Gold and Sela Brown will all look similar on new smooth wood.

Merbau and Red Iron Bark: Rred to brown tone so Autumntone, New Bronzetone, Merbau or Burnt Red will all look very similar on smooth wood.

Forest Reds and Jarrah: Red tones so Autumntone, New Bronzetone and Burnt Red are all close options and will look similar on smooth wood.

Changing the original colour of any wood

For horizontal walk on surfaces such as decking, we recommend you select a CUTEK® Colourtone that is the closest match to the wood you have selected, rather than attempt to change the colour. You can talk to any of our stockists for advice.

For cladding and screening, a much higher build of colour can be achieved which can completely change the original tone of the wood. Even very light wood coloured species can become an almost solid Black, Grey, Red, Brown or Gold if the wood surface is suitably rough and more coats or a higher pigment loading has been added.

In some circumstances you can double your CUTEK® Colourtone to achieve bolder effects on rough or brushed wood. We advise that you contact us to discuss this option in more detail as we want to ensure you have the best information possible.

Application

One CUTEK® colourtone size can be used in all pack sizes as follows:

  • 1 x 180 ml CUTEK® Colourtone pot is required for a 5 litre can of CUTEK® oil.
  • 2 x 180 ml CUTEK® Coloutone pots per 10 litre can of CUTEK® oil.
  • 4 x 180 ml CUTEK® Colourtone pots per 20 litre can of CUTEK® oil

Stir and mix the CUTEK® Colourtone well before adding into the clear oil. Continue to stir well with a flat stirrer, lifting from the bottom, for about 2 minutes before use and give a quick stir about every 15 minutes during use to ensure even results.

For best results, one coat of clear CUTEK® oil should be applied to all faces of the wood prior to installing, with a second and third coat of colourtoned CUTEK® oil applied to the top surface once the first coat is completely dry. Two or three thin coats on finished wood and hardwoods are better than one or two thick coats. CUTEK® oils will take longer to absorb/penetrate into dense hardwoods so thin coats are best so as to avoid delayed drying of the oil.

Maintenance

Colourtoned CUTEK® oil will lighten/fade faster in full weather exposed areas whereas wood in protected areas will retain colour with minimal maintenance over time.

CUTEK® is designed to gradually fade over time rather than peel, split or crack.  Rejuvenation of faded timbers coated with CUTEK® oils is a simple, fast and cost-effective process.

Clear or Colourtoned CUTEK® oil should be reapplied as frequently as necessary to retain the natural beauty and colour of the wood. Assessment of this is subjective and it is important to realise that colour durability varies widely according to many factors including the age and porosity of the wood, species, situation, exposure to the weather and how rough the wood surface is.

Typically, horizontal exterior wood surfaces exposed to full weather such as pool decks and handrails will require re-coating more frequently (initially after 6 months, then annually), while other surfaces such as vertical rough-sawn cladding will need recoating less often.

Use of CUTEK® Colourtones in non-CUTEK® products

It has come to our attention that representatives of other oil wood coatings are recommending the use of CUTEK® Colourtones in their own non-CUTEK® products. CUTEK® Colourtones are specially formulated for use in CUTEK® timber oils ONLY.

CUTEK® does not permit or endorse the use of CUTEK® Colourtones in any other third-party products.

Using CUTEK® exterior timber oils on Bamboo

As a substitute for hardwood floors bamboo can be an attractive choice. It looks great and as a renewable resource is an environmentally friendly option. Engineered bamboo offers stability and good looks too.

However, bamboo isn’t wood and behaves very differently. It needs a much higher level of care and a different approach to make sure it’s protected and stays looking its best for as long as possible.

We recommend using CUTEK® Extreme CD50 on bamboo. Other CUTEK® oils are not suitable for bamboo.

Bamboo is a grass, and doesn’t contain the extractives that give durability to many woods. It’s also very hygroscopic, meaning it takes up moisture rapidly and can also dry out very quickly, especially in direct sun. This makes engineered bamboo very susceptible to unsightly black staining moulds and significant surface erosion when exposed to rain and sun meaning that it will split/check and go grey/black rapidly if not properly protected.

Additionally, because engineered bamboo absorbs and releases moisture very quickly, most traditional wood coatings, deck stains and oils don’t last very long on fully weather exposed material.

We have observed that what may work reasonably well on wood for 6 to 12 months can often fail on bamboo material inside 12 weeks from time of application.

In our many years of testing, observation and user feedback, we have found that some engineered bamboo products are just not suitable for full weather exposed applications, despite manufacturer’s claims.

If you’re using CUTEK ® Extreme CD50 on bamboo we recommend following this process for best results.

It’s important to be aware that there are many engineered bamboo products on the market, of widely varying quality. CUTEK® Extreme CD50 may or may not work on your chosen engineered bamboo product despite following our recommendations.

  • Inspect your bamboo surface on a regular basis after coating and clean with CUTEK® Restore or CUTEK® QuickClean at the first sign of mould or surface erosion/splitting, followed by a reapplication of a thin coat of CUTEK® Extreme CD50. This must be done as frequently as is necessary.
  • If installing a bamboo deck that has been factory precoated with CUTEK® Extreme CD50 it will need at least one thin coat within one month of install. If mixing in a CUTEK® Colourtone to alter the existing colour, then two coats will be needed for adequate colour build. A further coat should be applied within 6 months, and another after 12 months.

New bamboo decking which has not been precoated with CUTEK® Extreme CD50 should be coated on all sides before installation, and given two further coats with a CUTEK® Colourtone within a month of installation, following the application procedure on the label.

A further coat should be applied within 6 months, and another after 12 months.

  • If using strand woven bamboo this product can contain glue which varies in quality. CUTEK® Extreme CD50 will not penetrate the glue in strand woven bamboo as it forms a physical barrier. Some products are very prone to surface expansion and become very rough. If this occurs, sanding back to a flat surface using 80 grit paper is the best preparation prior to application of CUTEK® Extreme CD50.

Clear CUTEK® Extreme CD50 can be used without a CUTEK® Colourtone, and will fade to a very light natural matt colour over a couple of months, but will resist greying for some time before needing to be recoated. To maintain a ‘freshly oiled’ look, more frequent oiling is required.

IMPORTANT NOTE

While the procedures detailed above have proven in some cases to produce a satisfactory result in the decorative coating of engineered bamboo in many countries and are detailed in good faith to assist people, we do not, and are unable to, offer any warranty or performance guarantee of any type (including but not limited to any warranty or performance guarantee in respect of coating longevity, mould/fungi degradation, and splitting/delamination) for the use of any CUTEK® products on any bamboo substrate.

This is due to the wide variation in the quality of products in the engineered bamboo market including variations in manufacturing processes, varying quality control, varying efficacy of preservative/treatment processes, origin of the raw bamboo, time of bamboo harvest, quality of the glues, place of manufacture etc.

Some manufacturers choose to specify CUTEK® oils as suitable for their engineered bamboo product, but this does not mean that we are included or involved in any independent warranties issued or implied by a specific manufacturer or distributor in relation to their product.

When should a colourtone be added to CUTEK® wood oils?

Un-tinted CUTEK® Extreme CD50 will quickly lighten/silver/grey with exposure to sunlight. Unless you want a clear finish that will naturally lighten/silver/grey off in a few months, it is important to mix in a CUTEK® Colourtones to CUTEK® oil before use. Adding CUTEK® Colourtones will provide UV colour protection and slows the lightening/silvering process.

NOTE: CUTEK® oils diffuse deeply into your timber and will continue to provide moisture protection and improve dimensional stability even if CUTEK® Colourtones are not added and your wood becomes weathered and greyed. To maintain your timber’s natural colour for longer, choose a CUTEK® Colourtone similar to the natural colour of your timber. Suggested CUTEK® Colourtones that match the natural hue of your timber can be found on our Colourtone product page. Colourtones can also help alter your timber colour if required (e.g. make your timber look lighter or darker than its natural state).

Order a from our website or your local stockist to test if your chosen Colourtone is right for your project.

NOTE: CUTEK® is unable to offer any specific performance warranties in relation to colour retention for CUTEK® products because of many variables related to the weathering process including but not limited to: the age and porosity of the wood, species, situation, design and structure, aspect, differing exposure to the weather and adequacy of preparation.

Wood Discolouration

Based on their causal factors and nature, wood discolourations can be put into two major groups, microbial and non-microbial discolourations. In our experience, non-microbial discolourations are not as well understood as microbial ones despite their common occurrence.

Microbial Colour Changes

Microbial discolourations are caused by micro-organisms. Many wood discolouring fungi/bacteria such as blue stain fungi, mould fungi, and bacteria, may produce dark or coloured stains when exposed to the right conditions of nutrient, moisture and light.

Non-microbial Colour Changes

Non-microbial discolourations can be mechanical (e.g., burn marks, dirt), chemical, biochemical or photochemical but may also have both chemical and microbial involvement. Analysis of these stains can be complex as many factors may be involved such as exposure to light and oxygen, substrate/coating pH, species, external contaminants, presence of metal ions and moisture content.

Discolouration and Extractives

All timber contains “extractives” which are chemicals that are solvent and/or water-soluble compounds that can be highly reactive. Extractives are non-structural chemical components that are mostly produced during heartwood formation. Extractives are extremely varied in their chemical nature and embrace many different classes of organic compounds, including tannins and other phenolic compounds, resins, essential oils, fats, terpenes, flavanoids, quinones, carbohydrates, glycosides and alkaloids.  These extractives can be a major contributor to timber discolourations. For example, some common polyphenol extractives exposed to oxygen and light, oxidise to form quinones and other complex polymers. Generally speaking, dark timbers tend to lighten and light-coloured wood tends to go yellow. Specific changes are very dependent on specific environmental conditions and species of timber.

Water Stain Discolouration

Exposure of raw wood to water can mobilize and cause leaching of water-soluble extractives presenting as unsightly water stain rings when the timber is dry. Water stain can be quickly and easily removed with CUTEK® Restore.

Natural Silvering of Wood

Uncoated exterior timbers that are exposed to UV sunlight breaks down the lignin in the cellulose causing photochemical degradation. This is what causes timber that is bare or coated in clear CUTEK® Extreme CD50 to lighten/silver over time. The specific shade of grey and rate of change is dependent on species, exposure aspect and coating format used. If you wish to slow the rate of “silvering off” of your exterior CUTEK® oil coated wood then it is vital to add a CUTEK® Colourtone to your CUTEK® Extreme CD50 oil prior to application in all coats. Exterior timber that has “greyed off” may be quickly and easily restored to fresh looking wood by using CUTEK® Restore.

Initial Colour Change Caused by the Application of CUTEK® Extreme CD50 to New Wood

CUTEK® Extreme CD50 applied to new timber can initially change the colour of the wood considerably, usually darkening the timber. This is due to the CUTEK® oil filling all the voids/pores in the timber and “wetting it out”. Typically, CUTEK® oil coated timbers will have a higher refractive value than air, hence the darker appearance upon initial coating. A quick and easy way to check what the colour of your freshly oiled CUTEK® wood will look like is to splash some water on the timber and observe the colour. Additionally, we can supply a to help you determine the suitability of colour for your own project.

Discolouration caused by Alkaline Materials

Alkaline substances and chemicals such as bleach and alkaline adhesives etc, can react with timbers high in polyphenolic tannins to produce stains. These resulting stains can often be distinguished from iron stain as they are usually brown in colour whereas iron stain typically has a black/blue appearance.

Discolouration Caused by Iron Stain

Iron stain is an unsightly blue–black or grey discoloration that is often incorrectly described as “mould” because of its frequently “spotty” appearance. Iron stain can occur on nearly all woods; however, some timbers are particularly prone to iron stain because they contain large amounts of tannin-like extractives. The discolouration is usually caused by a chemical reaction between extractives and iron content in steel products, such as nails, screws, and other fasteners. Steel used in contact with wood must be protected from corrosion by using stainless steel or processes such as hot dip galvanising. Problems with iron contamination can come from traces of iron left on wood from cutting, grinding or slicing; cleaning the surface with steel wool, wire brushes, or iron tools; using finishes stored in rusty containers; and using previous iron-containing or iron-contaminated finishes. Iron dust from metalworking and even plant fertilizers can be sources of iron along with removal of old rusted guttering, handrail construction and contact by steel capped boots. Merely striking wood with a hammer can cause iron stain on some timbers. Urine on wood floors will also hasten the reaction with iron and wood extractives, producing the typical iron stain discolouration. Unprotected timbers that get wet on or off site prior to fixing are particularly vulnerable as the water-soluble extractives are more readily mobilised to react with any iron contamination. Iron stain can be quickly and easily removed with CUTEK® Restore.

Discolouration in Timber with High Leucoanthocyanin Levels

Some timbers can contain high levels of naturally occurring tannins called leucoanthocyanins which normally appear colourless. In rare circumstances, the application of a higher acid value glue or coating (such as CUTEK® Extreme CD50) can cause the leucoanthocyanin tannin to chemically change into anthocyanins and other derivative compounds. These compounds can then appear in the visible region of the light spectrum, showing more commonly as an attractive red note enhancement of the underlying substrate, however more rarely purple, blue, bluish green through black hues may be visible in some areas. The actual colour of the stain is a function of overall pH and environmental factors such as heat, light levels, enzymes, and oxygen. Not all woods are susceptible.

Natural features of timber like this show why it is important to choose suitable timbers for the intended environment, coating format and end use application. If you suspect that this may be a problem for your project, order a to help determine the suitability of our products for your project.

Other Possible Discolourations of CUTEK® Exterior Oil Coated Timbers

CUTEK® Extreme CD50 contains a small amount of copper salts that may impart a faint green hue on some very light or white coloured timbers. This is more likely to occur in internal applications or in areas not exposed to UV light. Some commonly used light coloured timber species used internally where this may be an issue are Hoop Pine, Hemlock, Tasmanian Oak and Victorian Ash (list not exhaustive). We have a copper-free product called CUTEK® Euro (available by special order) which is extensively used as an alternative to CUTEK® Extreme CD50 in these instances . For more information regarding this option, please contact our friendly technical support team who will be able to assist you with your project.

To determine if CUTEK® Extreme CD50 or CUTEK® Euro is appropriate for your timber,  or contact us for further advice.

Remedial Treatments

CUTEK® are experts in remedial treatment products and processes for many types of wood discolourations and stains. If you have a specific issue that you would like advice on, please contact us for further information.

Clean Up with CUTEK®

As winter draws to a close and our homes are damp with moisture from the ongoing rain, mould and other fungal species are invading homes and timber decks.   To simplify your clean-up process, try CUTEK®…